Glue Chart by Frank Ford at Frets.com, from 1998. See also his HideGlueInfo page.
Source: GlueChart
© Frank Ford, 1998
Remember, these are opinions
Hide (hot) |
White/ Yellow |
Epoxy |
Cyanoacrylate | |
Heat Resistance |
high |
low |
low to med. |
high |
Gap Filling |
no |
no |
best |
good |
Water Cleanup |
best |
good |
no |
no |
Affect on finish |
no |
no |
sticks |
eats |
Tendency to Creep |
no |
yes |
varies |
no |
Runs into cracks |
good |
poor |
worst |
best |
Fingerboard |
best |
OK |
OK* |
OK* |
Bridge |
best |
good |
OK* |
OK* |
Top Braces |
best |
good |
OK* |
OK* |
Back Braces |
good |
best |
OK* |
OK* |
Dovetail |
good |
good |
NO** |
NO** |
Crack repair |
best |
good |
for open gaps only |
very tight cracks |
Deep Finish Fill |
no |
no |
good |
good |
Headstock crack |
good |
no |
OK |
good |
Inlay |
no |
no |
good |
best |
* The solvents in cyanoacrylate and those needed to clean up cyanoacrylate and epoxy are destructive to traditional lacquer, varnish and shellac finishes, making these glues poor choices for many applications. Most epoxy loses strength at the temperatures reached in hot parked cars, so it may not be the best choice for highly stressed applications around the bridge and neck.
** These glues make it impossible to disassemble dovetail neck joints!